Method a total quantity of iron ore of 10kg was split into equal parts using the rifflerne of these samples was used for screening on the 180 m sieve placed on the shaker and ran for 30 minutes reference sampleit was observed that for 2 and 4 minutes grind time, 14 and 14 fines and 85 and 85 coarse were produced.